I. Overview
In recent years, there has been a significant problem of "stage difference" in the verification and use of truck scales. These problems are mainly manifested in that. Some load-bearing devices composed of multi-section structures, as everyone imitates the U-beam structure in manufacturing, especially when welding U-beams.Without mastering the correct welding process in a continuous and uninterrupted manner, the accumulation of internal stress during processing occurred.Once released, it will cause the structure of the load-bearing device to deform, thereby affecting the measurement performance of the truck scale.
Ii. Welding Residual Stress and Deformation
During the welding process of steel structures, an uneven temperature field with local high temperatures is generated on the weldment, and the steel in the high-temperature part expands
The expansion is constrained by the adjacent steel, thereby causing high temperature stress and deformation inside the welded part, which is called welding stress.Welding deformation. The parts with higher welding stress will undergo plastic deformation, which will remain inside the component after cooling and thus remain
The welding stress and deformation within a component are called welding residual stress and welding residual deformation.
Welding residual stress.Welding residual stress is an internal stress without load, and thus it will self-balance within the component. Welding residue. Force includes longitudinal stress, transverse stress and stress in the thickness direction of the component.
① Longitudinal welding residual stress
Longitudinal welding stress refers to the stress along the length of the weld seam. During welding, an uneven temperature field is generated on the welded parts.
The temperature near the weld seam can reach over 1600℃, while the temperature in the adjacent area drops sharply. An uneven temperature field was generated
Uneven expansion: The steel expands most at the high-temperature area near the weld seam, while it expands less in the lower-temperature area. An area with significant expansion
The domain is restricted by the surrounding area with small expansion, resulting in thermoplastic compression. When the weld seam cools, thermoplastic compression occurs
The weld seam tends to shorten, but it is restricted by the steel on both sides, generating longitudinal tensile stress. The steel on both sides shrinks due to the middle weld seam
And longitudinal compressive stress is generated. Longitudinal residual stress of a Residual deformation of b welding; c Transverse residual stress (caused by longitudinal shrinkage); Transverse residual d
Residual stress (caused by lateral contraction) The total transverse residual stress of e
② Transverse welding residual stress
Transverse welding residual stress refers to the stress that is perpendicular to the length of the weld seam and parallel to the surface of the component. Welded with steel plates
For instance, the transverse welding residual stress consists of two parts: one part is the longitudinal contraction of the weld seam, which, in addition to generating the aforementioned longitudinal strain
In addition to the force, it also causes the two steel plates to tend to form bending deformations in opposite directions, but the weld seam has already joined them as a whole, so in the two Transverse tensile stress is generated in the middle of the block plate, and compressive stress is generated at both ends. Another part is due to the cooling of the weld seam during the welding process. The difference between them is that the weld seam welded first has solidified, which will prevent the subsequent weld seam from freely expanding laterally and cause it to undergo lateral compression. Plastic deformation. After the first welded part solidifies, the middle weld part gradually cools down, and the later welded part begins to cool down. These three parts. A lever effect is generated, causing the later welded part to contract and be stretched, the earlier welded part to also be stretched due to the lever effect, and the middle part to be compressed.And transverse welding residual stress is generated
③ Welding residual stress in the thickness direction
Welding residual stress in the thickness direction refers to the stress that is perpendicular to the length direction of the weld seam and also perpendicular to the surface of the component. Thicker steel
When welding plates, the cooling in the middle of the weld thickness direction is slower than that on the surface, resulting in a state where the middle weld is under tension and the periphery is under compression.
Therefore, in addition to longitudinal and transverse stresses, there is also welding residual stress in the thickness direction of the weld seam.residual stress is an internal stress in self-equilibrium, and the resultant force of tensile stress is equal to that of compressive stress. Therefore, for welded components without strict stress concentration, under static loading, as long as the steel has a certain plastic deformation capacity,Welding residual stress does not affect the load-bearing capacity of components.